Rods, Bar and Wire
Rods
Rod is a product made from the stainless steel material and are used as per the different grades available as per the industries, These bars are known for their strength and corrosion resistance properties.
These bars are used in aesthetic applications and outdoor fixtures, Cold drawn steel bars are preferred as it has smooth surface and less absolute roughness. These bars vary in sizes.
Below are the Compositions for 2 different bars.s
We also stock Bar, Hexagon, Square, Round
products in various dimensions and
grades.
We stock Stainless Steel, carbon and alloy
specialty steels supplied in the as rolled,
annealed and normalized conditions. We offer
cut to size and heat treatment through our
service center.
User Industries:
Chemicals, Fats, & Fertilizers, Sugar
Mills & Distilleries, Cement Industries,
Ship Builders, Paper Industries, Pumps,
Petrochemicals, Oil & Natural Gas
Organization in terms of the specific
materials, Technology, Finance &
Personal.
Product Range:
The following table represents size range,
product standards and material grades of
Round Bars.
| Stainless & Duplex Steel | |
|---|---|
| Range | 3.17 MM TO 350 MM DIA |
| Stainless Steel | ASTM / ASME SA 276 TP 304 , 304L
, 309S , 309H, 310S , 316 , 316L
, 316 TI , 317 , 321 , 347 , 410
, 420 , 430 ,431 , 440A ,B &
C. , 446
ASTM / ASME SA 479 TP 304 , 304L , 304H, 309S , 309H, 310S , 310H , 316 , 316H , 316L , 316 TI , 317 , 321 , 321H , 347 , 347 H , 410, 430 ,431 & 444. |
| Duplex Steel | ASTM / ASME SA 276 UNS NO. S 31803 , S 32205 , S 32550 , S 32750 , S 32760 |
| Nickel & Copper Alloy | |
|---|---|
| Range | 3.17 MM TO 350 MM DIA |
| Nickel Alloy | ASTM / ASME SB 160 UNS 2200 (
NICKEL 200 ) / UNS 2201 (NICKEL
201 )
ASTM / ASME SB 164 UNS 4400 (MONEL 400 ) ASTM / ASME SB 425 UNS 8825 (INCONEL 825) ASTM / ASME SB 166 UNS 6600 (INCONEL 600 ) / UNS 6601 ( INCONEL 601 ) ASTM / ASME SB 446UNS 6625 (INCONEL 625) ASTM / ASME SB 574 UNS 10276 ( HASTELLOY C 276 ) ASTM / ASME SB 472 UNS 8020 ( ALLOY 20 / 20 CB 3 ) |
| Carbon & Alloy Steel | |
|---|---|
| Range | 3.17 MM TO 350 MM DIA |
| Carbon Steel | ASTM / ASME A 105 |
| Alloy Steel | ASTM / ASME A 182 GR F 5, F 9 ,
F 11 , F 12 , F 22 , F 91.
ASTM / ASME A 729 GR B 11 & B 22. |
Chemical Composition for Stainless Steel Bars
| ASTM Grade | Carbon | Manganese | Silicon | Sulfur | Phospherous | Chromium | Nickel | Molybdenum | Other |
|---|---|---|---|---|---|---|---|---|---|
| 304 | 0.08 max | 2.00 max | 0.75 max | 0.030 max | 0.045 max | 18.0-20.0 | 8.0 11.0 | – | – |
| 316 | 0.08 max | 2.00 max | 0.75 max | 0.030 max | 0.045 max | 16.0-18.0 | 10.0 14.0 | 2.0 3.0 | – |
| 317L | 0.035 max | 2.00 max | 0.75 max | 0.030 max | 0.045 max | 18.0-20.0 | 11.0 14.0 | 3.0 4.0 | – |
| 310 S | 0.08 max | 2.00 max | 1.5 max | 0.030 max | 0.045 max | 24.0-26.0 | 19.0 22.0 | 3.0 4.0 | – |
| 347 H | 0.04 0.10 | 2.00 max | 0.75 max | 0.030 max | 0.045 max | 17.0- 19.0 | 9.0 13.0 | – | 10C(Cb+Ta)<1.10% |
| 321 | 0.08 | 2.00 max | 0.75 max | 0.030 max | 0.045 max | 17.0-20.0 | 9.0 12.0 | – | 5C 0.70% |
Mechanical Analysis of Stainless Steel Bars
| Grade | Elongation | Density | Tensile Strength | Yield Strength (0.2%Offset) | Melting Point |
|---|---|---|---|---|---|
| SS 202 | 40 % | 8.0 g/cm3 | 515 MPa | 275 MPa | 1454 °C (2650 °F) |
| SS 303 | 50 % | 55% | Psi – 85,000 | Psi – 45,000 | Rb 180 |
| SS 304 | 40% | 8.0 g/cm3 | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 1400 °C (2550 °F) |
| SS 304L | 40% | 8.0 g/cm3 | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 1400 °C (2550 °F) |
| SS 316 | 35 % | 8.0 g/cm3 | Psi – 75000 , MPa – 515 | Psi – 30000 , MPa – 205 | 1454 °C (2650 °F) |
| SS 316L | 40 % | 8.0 g/cm3 | 485 Min | 170 Min. | 1400 °C (2550 °F) |